Major Rust Repair

Discussion in 'Cosmetic' started by Racer_X, Mar 29, 2012.

  1. Resto

    Resto Benders Evil Twin

    Joined:
    Sep 2, 2010
    Messages:
    1,293
    Likes Received:
    5
    Trophy Points:
    147
    Location:
    Yuma AZ
    Vehicle:
    73 Mav Buckets(69 351W, soon to be 408) Floorshift FXBDY AOD ,07 Glide,06 E250HA,01 Silverado
    All Great counsel Bros. Im a Tac Tac Tac fan. I dont stay on the triger for more than 1.5 seconds and less than that with the real thin metal. I leave a gap between the patch and the patchee the width of the wire Im useing mostly .030 and place the wire in the gap and hit the trigger, then move away from that tac so it cools after the 1st couple tacs I break out my copper spoon.Some times if Im in a thin spot I keep my air gun handy and as soon as I tac I hit the tac with a burst of air. Id practice on some thin scrap 1st till you can get to know what it takes to make holes and adjust your technique. Good Luck(y)
     
  2. Mysidekickgoose

    Mysidekickgoose Member

    Joined:
    Apr 13, 2011
    Messages:
    117
    Likes Received:
    3
    Trophy Points:
    45
    Location:
    Knoxville, TN
    Vehicle:
    1974 ford maverick 4-speed automatic I6, 94' Toyota Celica FWD I4 5-speed manual, 84' Toyota Celica RWD 2.4L I4 5-speed manual
    rest in peace. lol
     
  3. Joe Dirt

    Joe Dirt BBF life

    Joined:
    Dec 16, 2008
    Messages:
    4,375
    Likes Received:
    7
    Trophy Points:
    172
    Location:
    Cleveland, TN
    Vehicle:
    1970 ford torino #1
    Thin gauge wire and low heat will help from burning through thin metal
     
  4. WeekendWarrior

    WeekendWarrior Member

    Joined:
    Jan 9, 2012
    Messages:
    39
    Likes Received:
    0
    Trophy Points:
    0
    Location:
    southeast georgia
    Vehicle:
    1976 ford maverick
    dang, the rear bumper appears be better shape then mine, id love have some them chrome trim work too :biglaugh:
     